Machining of Metal-Matrix Composites and Honeycomb Structures

By
Harry E. Chandler
Harry E. Chandler
ASM International
Search for other works by this author on:
Published:
1989
Page range:
893 - 901

Abstract

This article presents general guidelines for machining metal matrix composites (MMC) and honeycomb structures. It provides guidelines for machining of specific MMCs, namely, aluminum-boron, aluminum-SiC, aluminum-Al2O3, and titanium-SiC MMCs. In addition, the article discusses the various parameters influencing drilling of dissimilar-material laminates.

You do not currently have access to this content.
Don't already have an account? Register

Harry E. Chandler, 1989. "Machining of Metal-Matrix Composites and Honeycomb Structures", Machining

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal