Abstract

This article discusses the principal process steps, specifications, defects, applications, advantages, and disadvantages of chemical milling (CM) in aerospace industries. The process steps include precleaning, masking, scribing, etching, final cleaning, stripping, and mechanical finishing. The article describes the variables that affect undercut and surface finish obtained by CM. The mechanical properties of chemically milled parts are also discussed.

You do not currently have access to this content.
Don't already have an account? Register

Eugene M. Langworthy, 1989. "Chemical Milling", Machining

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal