Abstract

This article discusses various machining techniques of zinc alloy die castings. These include turning, boring, drilling, reaming, tapping, die threading, milling, and sawing. In addition, the article describes the factors that influence machinability of the zinc alloy die castings.

You do not currently have access to this content.
Don't already have an account? Register

Gary Adams, 1989. "Machining of Zinc Alloy Die Castings", Machining, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal