Book Chapter

Lapping

By
Pel Lynah
Pel Lynah
Revising author
P.R. Hoffman Machine Products
Search for other works by this author on:
Published:
1989
Page range:
492 - 505

Abstract

Lapping is the lower-pressure, lower-speed, and lower-power application of the use of fixed abrasives. This article begins with a discussion on the process capabilities of lapping and reviews the selection of abrasive and vehicle for lapping. It describes the methods of lapping outer cylindrical surfaces, namely, ring lapping, machine lapping between plates, centerless roll lapping with loose abrasives, and centerless lapping with bonded abrasives. In addition, the article discusses the methods employed for lapping of outer surfaces of piston rings, crankshafts, inner cylindrical surfaces, flat surfaces, end surfaces, spherical surfaces, balls, spring like parts, and gears. It also reviews the problems in flat and end lapping. The article concludes information on the use of lapping in accelerated wearing-in process for matching and aligning components of bearing assemblies.

You do not currently have access to this content.
Don't already have an account? Register

Pel Lynah, 1989. "Lapping", Machining, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal