Skip to Main Content
ASM Handbook

Machining

By
ASM Handbook Committee
ASM Handbook Committee
Search for other works by this author on:
ASM International
Volume
16
ISBN electronic:
978-1-62708-188-7
Publication date:
1989
Book Chapter

P/M High-Speed Tool Steels

By
Kenneth E. Pinnow
Kenneth E. Pinnow
Revising author
Crucible Materials Corporation
Search for other works by this author on:
William Stasko
William Stasko
Revising author
Crucible Materials Corporation
Search for other works by this author on:
Published:
1989
Page range:
60 - 68

Abstract

This article describes procedures for producing powder metallurgy high-speed tool steel powder by inert-gas atomization, followed by compaction by hot isostatic pressing. These include the anti-segregation process (ASP) and the crucible particle metallurgy (CPM) process. The article reviews the properties of ASP and CPM and summarizes the procedures to heat treat ASP high-speed tool steels. It discusses the processing steps, advantages, and applications of the FULDENS process that uses water-atomized powders compacted by vacuum sintering. The article also provides information on the applications of tool steels.

You do not currently have access to this content.
Don't already have an account? Register

Kenneth E. Pinnow, William Stasko, 1989. "P/M High-Speed Tool Steels", Machining, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal