Electrostream and Capillary Drilling

By
M. Anthony Newton
M. Anthony Newton
Nltech, Inc.
Search for other works by this author on:
Published:
1989
Page range:
551 - 553

Abstract

This article describes the applications, process capabilities, and limitations and advantages of electrostream and capillary drilling. It describes equipment and tooling used for electrostream and capillary drilling. These include electrostream and capillary drilling machines, power supplies, electrolyte system, part holding fixtures, cathode holders, and cathode tubes. Key process parameters for electrostream and capillary drilling are also discussed.

You do not currently have access to this content.
Don't already have an account? Register

M. Anthony Newton, 1989. "Electrostream and Capillary Drilling", Machining, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal