Machining of Uranium and Uranium Alloys

By
James A. Aris
James A. Aris
Rockwell International
Search for other works by this author on:
Published:
1989
Page range:
874 - 878

Abstract

This article focuses on the basic metallurgy and machining parameters of classes of depleted and enriched uranium alloys. It provides information on the health precautions applicable to the machining of depleted uranium alloys. The article also discusses tool wear and the types of tools used in uranium alloy machining.

You do not currently have access to this content.
Don't already have an account? Register

James A. Aris, 1989. "Machining of Uranium and Uranium Alloys", Machining, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal