Skip to Main Content
ASM Handbook

Machining

By
ASM Handbook Committee
ASM Handbook Committee
Search for other works by this author on:
ASM International
Volume
16
ISBN electronic:
978-1-62708-188-7
Publication date:
1989
Book Chapter

Machining of Beryllium[1]

By
Douglas V. Gallagher
Douglas V. Gallagher
Rockwell International
Search for other works by this author on:
R.E. Hardesty
R.E. Hardesty
Electrofusion Corporation
Search for other works by this author on:
Published:
1989
Page range:
870 - 873

Abstract

This article discusses the properties of beryllium metals that require special attention when machining. It provides information on the considerations of S65 and selects 65 beryllium materials that are used for conducting tool wear studies and surface damage studies. The article highlights some of the precautions to be followed while machining beryllium metals. Information on the cutting oils, cutting tools, and speeds and feeds used in turning the beryllium are also provided. The article describes the chemical milling and photochemical machining methods that are used for etching beryllium components.

You do not currently have access to this content.
Don't already have an account? Register

Douglas V. Gallagher, R.E. Hardesty, 1989. "Machining of Beryllium", Machining, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal