Book Chapter

Machining of Stainless Steels

By
Ted Kosa
Ted Kosa
Carpenter Technology Corporation
Search for other works by this author on:
Ronald P. Ney, Sr.
Ronald P. Ney, Sr.
Carpenter Technology Corporation
Search for other works by this author on:
Published:
1989
Page range:
681 - 707

Abstract

The machinability of stainless steels varies from low to very high, depending on the final choice of the alloy. This article discusses general material and machining characteristics of stainless steel. It briefly describes the classes of stainless steel, such as ferritic, martensitic, austenitic, duplex, and precipitation-hardenable alloys. The article examines the role of additives, such as sulfur, selenium, tellurium, lead, bismuth, and certain oxides, in improving machining performance. It provides ways to minimize difficulties involved in the traditional machining of stainless steels. The article describes turning, drilling, tapping, milling, broaching, reaming, and grinding operations on stainless steel. It concludes with information on some of the nontraditional machining techniques, including abrasive jet machining, abrasive waterjet machining electrochemical machining, electron beam machining, and plasma arc machining.

You do not currently have access to this content.
Don't already have an account? Register

Ted Kosa, Ronald P. Ney, Sr., 1989. "Machining of Stainless Steels", Machining, ASM Handbook Committee