Abstract

This article focuses on the machining of reactive metals which refer collectively to the elements titanium, hafnium, and zirconium. It provides guidelines for machining titanium and titanium alloys and describes machining operations, such as turning, milling, drilling, tapping, reaming, grinding, and sawing, performed on titanium and its alloys. The article also provides information on electrochemical machining (ECM), chemical milling (CHM), and laser beam machining (LBM) for titanium and titanium alloys. Guidelines for machining zirconium alloys and hafnium are also provided. The article provides a short description of turning, milling, and drilling operations performed on zirconium alloys and hafnium. It also discusses health and safety considerations related to zirconium and hafnium.

You do not currently have access to this content.
Don't already have an account? Register

Harry E. Chandler, 1989. "Machining of Reactive Metals", Machining, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal