Abstract

This article discusses the classifications of high-speed tool steels and describes alloying elements and their effects on the properties of high-speed tool steels. It analyzes the heat treatment of high-speed tool steels, namely, preheating, austenitizing, quenching, and tempering. Surface treatments for the high-speed tool steels are reviewed. The article emphasizes the properties and applications of high-speed tool steels and provides information on the factors in selecting high-speed tool steels.

Abstract

This article describes procedures for producing powder metallurgy high-speed tool steel powder by inert-gas atomization, followed by compaction by hot isostatic pressing. These include the anti-segregation process (ASP) and the crucible particle metallurgy (CPM) process. The article reviews the properties of ASP and CPM and summarizes the procedures to heat treat ASP high-speed tool steels. It discusses the processing steps, advantages, and applications of the FULDENS process that uses water-atomized powders compacted by vacuum sintering. The article also provides information on the applications of tool steels.

You do not currently have access to this content.
Don't already have an account? Register

1989. "Cutting Tool Materials", Machining, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal