Book Chapter

Thermomechanical Testing[1]

By
St├ęphane Guillard
Stéphane Guillard
Concurrent Technologies Corporation
Search for other works by this author on:
Koushik Ray
Koushik Ray
Concurrent Technologies Corporation
Search for other works by this author on:
Published:
2005
Publication history
March 09, 2009

Abstract

Thermomechanical are used to gain insight into the causes of problems that arise during a given thermomechanical process. This article provides examples to demonstrate how significant the parameters were selected for specific tests. It examines the types of problems that can occur during a thermomechanical process. The article provides information on the thermophysical properties, which include specific heat, coefficient of thermal expansion, thermal conductivity/diffusivity, and density. It concludes with examples that illustrate how the various considerations in testing are successfully used to solve practical thermomechanical processing problems.

You do not currently have access to this content.
Don't already have an account? Register

St├ęphane Guillard, Koushik Ray, 2005. "Thermomechanical Testing", Metalworking: Bulk Forming, S.L. Semiatin