Hot-Compression Testing[1]

By
George E. Dieter
George E. Dieter
University of Maryland
Search for other works by this author on:
Published:
2005
Publication history
March 09, 2009

Abstract

This article describes the use of compression tests, namely, cylindrical compression, ring compression, and plane-strain compression tests at elevated temperatures. It discusses the effects of the temperature, strain rate, and deformation heating on metals during the cylindrical compression test, with the help of flow curves. The article illustrates the testing apparatus used in the cylindrical compression test. It describes the issues regarding friction and temperature, and strain-rate control with proper test equipment and experimental planning during the ring compression test and plane-strain compression test. The article also reviews the testing conditions, procedures, and advantages of hot plane-strain compression test.

You do not currently have access to this content.
Don't already have an account? Register

George E. Dieter, 2005. "Hot-Compression Testing", Metalworking: Bulk Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal