Useful Formulas for Deformation Analysis and Workability Testing

Published:
2005
Page range:
827 - 830
Publication history
April 03, 2006

Abstract

This article contains nine tables that present useful formulas for deformation analysis and workability testing. The tables present formulas for effective stress, strain, and strain rate in arbitrary coordinates, principal, compression and tension testing of isotropic material. The article also provides formulas for flat rolling, conical-die extrusion, wire drawing, deep drawing of cups from sheet metal, and bending, and formulas for anisotropic sheet materials.

You do not currently have access to this content.
Don't already have an account? Register

2005. "Useful Formulas for Deformation Analysis and Workability Testing", Metalworking: Bulk Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal