Coining

Published:
2005
Page range:
198 - 204
Publication history
March 21, 2006

Abstract

Coining is a closed-die forging operation in which all surfaces of the workpiece are confined or restrained, resulting in a well-defined imprint of the die on the workpiece. This article focuses on the coining equipment (hammers and presses), lubricants, and general and special die materials used in the coining process. It discusses the coinability of metals such as steels, copper, and composite metals. The article describes the control of dimensions, surface finishes, and weight of coined items. It concludes with a discussion on processing problems and solutions.

You do not currently have access to this content.
Don't already have an account? Register

2005. "Coining", Metalworking: Bulk Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal