Skip to Main Content
ASM Handbook

Metalworking: Bulk Forming

Edited by
S.L. Semiatin
S.L. Semiatin
Search for other works by this author on:
ASM International
Volume
14A
ISBN electronic:
978-1-62708-185-6
Publication date:
2005
Book Chapter

Forging of Refractory Metals

By
John A. Shields, Jr.
John A. Shields, Jr.
H.C. Starck, Inc.
Search for other works by this author on:
Kurt D. Moser
Kurt D. Moser
H.C. Starck, Inc.
Search for other works by this author on:
R. William Buckman, Jr.
R. William Buckman, Jr.
Refractory Metals Technology
Search for other works by this author on:
Todd Leonhardt
Todd Leonhardt
Rhenium Alloys
Search for other works by this author on:
C. Craig Wojcik
C. Craig Wojcik
Allegheny Wah Chang
Search for other works by this author on:
Published:
2005
Page range:
284 - 285
Publication history
March 22, 2006

Abstract

This article focuses on the forging characteristics of different types of refractory metals and alloys, namely, niobium and niobium alloys, molybdenum and molybdenum alloys, tantalum and tantalum alloys, and tungsten and tungsten alloys.

You do not currently have access to this content.
Don't already have an account? Register

John A. Shields, Jr., Kurt D. Moser, R. William Buckman, Jr., Todd Leonhardt, C. Craig Wojcik, 2005. "Forging of Refractory Metals", Metalworking: Bulk Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal