Book Chapter

Isothermal and Hot-Die Forging

By
R.E. Montero
R.E. Montero
Revising author
Pratt & Whitney
Search for other works by this author on:
L.G. Housefield
L.G. Housefield
Revising author
Pratt & Whitney
Search for other works by this author on:
R.S. Mace
R.S. Mace
Revising author
Pratt & Whitney
Search for other works by this author on:
Published:
2005
Page range:
183 - 192
Publication history
March 21, 2006

Abstract

Hot-die forging and isothermal forging are unique forging methods developed to forge materials that are difficult or impossible to forge by conventional means. This article presents a comparative study on hot-die forging and isothermal forging. It discusses forging parameters, process selection considerations, design guidelines, alloy types and selection, and the advantages and disadvantages of hot-die forging and isothermal forging. The article discusses the application of the finite-element analysis modeling to design.

You do not currently have access to this content.
Don't already have an account? Register

R.E. Montero, L.G. Housefield, R.S. Mace, 2005. "Isothermal and Hot-Die Forging", Metalworking: Bulk Forming, S.L. Semiatin