Abstract

The drawing process, one of the oldest metal forming operations, allows excellent surface finishes and closely controlled dimensions to be obtained in long products that have constant cross sections. This article discusses the basic mechanics and preparation steps of drawing. It presents an overview of the processes, equipment, dies and die materials, and lubrication associated with drawing of rod, wire, bar, and tube. The article also provides a discussion on the design considerations and manufacturing of commercial superconducting multifilamentary conductors.

You do not currently have access to this content.
Don't already have an account? Register

2005. "Wire, Rod, and Tube Drawing", Metalworking: Bulk Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal