Bulk Workability of Metals[1]

By
George E. Dieter
George E. Dieter
University of Maryland
Search for other works by this author on:
Published:
2005
Page range:
1 - 14
Publication history
March 09, 2009

Abstract

This article provides the definitions of stress and strain, and describes the relationship between stress and strain by stress-strain curves and true-stress/true-strain curves. The emphasis is on understanding the factors that determine the extent of deformation a metal can withstand before cracking or fracture occurs. The article reviews the process variables that influence the degree of workability and summarizes the mathematical relationships that describe the occurrence of room-temperature ductile fracture under workability conditions. It discusses the most common situations encountered in multiaxial stress states. The construction of a processing map based on deformation mechanisms is also discussed.

You do not currently have access to this content.
Don't already have an account? Register

George E. Dieter, 2005. "Bulk Workability of Metals", Metalworking: Bulk Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal