Skip to Main Content
ASM Handbook

Metalworking: Bulk Forming

Edited by
S.L. Semiatin
S.L. Semiatin
Search for other works by this author on:
ASM International
Volume
14A
ISBN electronic:
978-1-62708-185-6
Publication date:
2005
Book Chapter

Workpiece Materials Database

By
St├ęphane Guillard
Stéphane Guillard
Concurrent Technologies Corporation
Search for other works by this author on:
Published:
2005
Page range:
651 - 659
Publication history
February 14, 2005

Abstract

The material data for forging can be divided into two categories, namely, mechanical properties and thermophysical properties. This article describes the flow characteristics of key engineering materials, such as steels, aluminum alloys, copper alloys, titanium alloys, and nickel-base superalloys. It discusses the thermophysical properties for designing or optimizing a metalworking process: specific heat, coefficient of thermal expansion, thermal conductivity/diffusivity, and density.

You do not currently have access to this content.
Don't already have an account? Register

St├ęphane Guillard, 2005. "Workpiece Materials Database", Metalworking: Bulk Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal