Skip to Main Content
ASM Handbook

Metalworking: Bulk Forming

Edited by
S.L. Semiatin
S.L. Semiatin
Search for other works by this author on:
ASM International
Volume
14A
ISBN electronic:
978-1-62708-185-6
Publication date:
2005
Book Chapter

Hydrostatic Extrusion of Metals and Alloys

By
J.J. Lewandowski
J.J. Lewandowski
Case Western Reserve University
Search for other works by this author on:
A. Awadallah
A. Awadallah
Case Western Reserve University
Search for other works by this author on:
Published:
2005
Page range:
440 - 447
Publication history
February 17, 2006

Abstract

This article begins with a general review of the effects of changes in stress state on processing of materials. It describes the fundamentals of hydrostatic extrusion and reviews the various issues and benefits associated with hydrostatic extrusion. The article discusses the hydrostatic extrusion of structural alloys, composites, brittle materials, and intermetallics or intermetallic compounds, with examples. It concludes with a discussion on the attempts made to extend the hydrostatic extrusion to higher temperatures.

You do not currently have access to this content.
Don't already have an account? Register

J.J. Lewandowski, A. Awadallah, 2005. "Hydrostatic Extrusion of Metals and Alloys", Metalworking: Bulk Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal