Skip to Main Content
ASM Handbook

Metalworking: Bulk Forming

Edited by
S.L. Semiatin
S.L. Semiatin
Search for other works by this author on:
ASM International
Volume
14A
ISBN electronic:
978-1-62708-185-6
Publication date:
2005
Book Chapter

Bulk Workability Testing[1]

By
George E. Dieter
George E. Dieter
University of Maryland
Search for other works by this author on:
Published:
2005
Page range:
1 - 11
Publication history
November 15, 2008

Abstract

This article discusses a number of workability tests that are especially applicable to the forging process. The primary tests for workability are those for which the stress state is well known and controlled. The article provides information on the tension test, torsion test, compression test, and bend test. It examines specialized tests including plane-strain compression test, partial-width indentation test, secondary-tension test, and ring compression test. The article explains that workability is determined by two main factors: the ability to deform without fracture and the stress state and friction conditions present in the bulk deformation process. These two factors are described and brought together in an experimental workability analysis.

You do not currently have access to this content.
Don't already have an account? Register

George E. Dieter, 2005. "Bulk Workability Testing", Metalworking: Bulk Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal