Forging of Titanium Alloys

By
G.W. Kuhlman
G.W. Kuhlman
Metalworking Consultant Group LLC
Search for other works by this author on:
Published:
2005
Page range:
331 - 353
Publication history
March 28, 2006

Abstract

Titanium alloys are forged into a variety of shapes and types of forgings, with a broad range of final part forging design criteria based on the intended end-product application. This article begins with a discussion on the classes of titanium alloys, their forgeability, and factors affecting forgeability. It describes the forging techniques, equipment, and common processing elements associated with titanium alloy forging. The processing elements include the preparation of forging stock, preheating of the stock, die heating, lubrication, forging process, trimming and repair, cleaning, heat treatment, and inspection. The article presents a discussion on titanium alloy precision forgings and concludes with information on the forging of advanced titanium materials and titanium aluminides.

You do not currently have access to this content.
Don't already have an account? Register

G.W. Kuhlman, 2005. "Forging of Titanium Alloys", Metalworking: Bulk Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal