Equal-Channel Angular Extrusion

By
Vladimir Segal
Vladimir Segal
Engineered Performance Materials Co.
Search for other works by this author on:
Published:
2005
Page range:
528 - 536
Publication history
March 27, 2006

Abstract

This article describes the mechanics and processing characteristics of equal-channel angular extrusion (ECAE). Tool design considerations for the ECAE are discussed. During ECAE, severe plastic strains and simple shear deformation mode contribute to strong, sometimes unusual effects of processing on structure and properties. The article explains these effects and concludes with a discussion on the applications of the ECAE.

You do not currently have access to this content.
Don't already have an account? Register

Vladimir Segal, 2005. "Equal-Channel Angular Extrusion", Metalworking: Bulk Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal