Roll Forging

By
Prabir K. Chaudhury
Prabir K. Chaudhury
Orbital Sciences Corporation
Search for other works by this author on:
Roger Rees
Roger Rees
Forging Division, SMS Eumuco Inc.
Search for other works by this author on:
Published:
2005
Page range:
131 - 135
Publication history
March 20, 2006

Abstract

Roll forging is a process for simultaneously reducing the cross-sectional area and changing the shape of heated bars, billets, or plates. This article provides an overview of the process capabilities, production techniques, machines and machine size selection considerations, and types of roll dies and auxiliary tools for the roll forging. It concludes with information on the production examples of roll forging.

You do not currently have access to this content.
Don't already have an account? Register

Prabir K. Chaudhury, Roger Rees, 2005. "Roll Forging", Metalworking: Bulk Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal