Skip to Main Content
ASM Handbook

Metalworking: Bulk Forming

Edited by
S.L. Semiatin
S.L. Semiatin
Search for other works by this author on:
ASM International
Volume
14A
ISBN electronic:
978-1-62708-185-6
Publication date:
2005
Book Chapter

Hot Upset Forging

By
J. Richard Douglas
J. Richard Douglas
Revising author
Metalworking Consultant Group LLC
Search for other works by this author on:
Published:
2005
Page range:
119 - 130
Publication history
March 20, 2006

Abstract

This article discusses the operation of upset forging machines and selection of the machine size. It describes several types of upsetter heading tools and their materials. The article reviews the cold shearing and hot shearing methods for preparing blanks for hot upset forging. It deals with various upsetting processes: offset upsetting, double-end upsetting, upsetting with sliding dies, upsetting pipe and tubing, and electric upsetting. The article also provides information on hot forging and cold forging.

You do not currently have access to this content.
Don't already have an account? Register

J. Richard Douglas, 2005. "Hot Upset Forging", Metalworking: Bulk Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal