Introduction to Bulk-Forming Processes

By
S.L. Semiatin
S.L. Semiatin
Air Force Research Laboratory, Materials and Manufacturing Directorate
Search for other works by this author on:
Published:
2005
Page range:
3 - 10
Publication history
February 28, 2006

Abstract

Metalworking is one of the three major technologies used to fabricate metal products. This article tabulates the classification of metal forming processes. It discusses different types of metalworking equipment, including rolling mills, ring-rolling machines, and thread-rolling and surface-rolling machines. The article outlines the significant characteristics of pressing-type machines: load and energy characteristics, time-related characteristics, and accuracy characteristics. It summarizes different specialized processes such as advanced roll-forming methods, equal-channel angular extrusion, incremental forging, and microforming. The article describes the thermomechanical processing of nickel- and titanium-base alloys and concludes with information on the advancements in process simulation.

You do not currently have access to this content.
Don't already have an account? Register

S.L. Semiatin, 2005. "Introduction to Bulk-Forming Processes", Metalworking: Bulk Forming, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal