Book Chapter

Wear Failures of Reinforced Polymers

By
J. Bijwe
J. Bijwe
Indian Institute of Technology
,
Delhi
Search for other works by this author on:
Published:
2002
Page range:
1028 - 1043
Publication history
November 01, 2002

Abstract

This article reviews the abrasive and adhesive wear failure of several types of reinforced polymers, including particulate-reinforced polymers, short-fiber reinforced polymers (SFRP), continuous unidirectional fiber reinforced polymers (FRP), particulate-filled composites, mixed composites (SFRP and particulate-filled), unidirectional FRP composites, and fabric reinforced composites. Friction and wear performance of the composites, correlation of performance with various materials properties, and studies on wear-of failure mechanisms by scanning electron microscopy are discussed for each of these types.

You do not currently have access to this content.
Don't already have an account? Register

J. Bijwe, 2002. "Wear Failures of Reinforced Polymers", Failure Analysis and Prevention, William T. Becker, Roch J. Shipley

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal