Skip to Main Content
ASM Handbook

Failure Analysis and Prevention

Edited by
William T. Becker
William T. Becker
Search for other works by this author on:
Roch J. Shipley
Roch J. Shipley
Search for other works by this author on:
ASM International
Volume
11
ISBN electronic:
978-1-62708-180-1
Publication date:
2002
Book Chapter

Introduction to Failure Analysis and Prevention

By
James J. Scutti
James J. Scutti
Massachusetts Materials Research, Inc.
Search for other works by this author on:
William J. McBrine
William J. McBrine
ALTRAN Corporation
Search for other works by this author on:
Published:
2002
Page range:
3 - 23
Publication history
November 01, 2002

Abstract

This article briefly introduces the concepts of failure analysis and root cause analysis (RCA), and the role of failure analysis as a general engineering tool for enhancing product quality and failure prevention. It reviews four fundamental categories of physical root causes, namely, design deficiencies, material defects, manufacturing/installation defects, and service life anomalies, with examples. The article describes several common charting methods that may be useful in performing an RCA. It also discusses other failure analysis tools, including review of all sources of input and information, people interviews, laboratory investigations, stress analysis, and fracture mechanics analysis. The article concludes with information on the categories of failure and failure prevention.

You do not currently have access to this content.
Don't already have an account? Register

James J. Scutti, William J. McBrine, 2002. "Introduction to Failure Analysis and Prevention", Failure Analysis and Prevention, William T. Becker, Roch J. Shipley

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal