Forms of Corrosion

Published:
2002
Page range:
761 - 795
Publication history
November 01, 2002

Abstract

This article addresses the forms of corrosion that contribute directly to the failure of metal parts or that render them susceptible to failure by some other mechanism. It describes the mechanisms of corrosive attack for specific forms of corrosion such as galvanic corrosion, uniform corrosion, pitting and crevice corrosion, intergranular corrosion, and velocity-affected corrosion. The article contains a table that lists combinations of alloys and environments subjected to selective leaching and the elements removed by leaching.

You do not currently have access to this content.
Don't already have an account? Register

2002. "Forms of Corrosion", Failure Analysis and Prevention, William T. Becker, Roch J. Shipley

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal