Fracture Appearance and Mechanisms of Deformation and Fracture

By
W.T. Becker
W.T. Becker
University of Tennessee, Emeritus
Search for other works by this author on:
S. Lampman
S. Lampman
ASM International
Search for other works by this author on:
Published:
2002
Page range:
559 - 586
Publication history
November 01, 2002

Abstract

This article provides an overview of fractography and explains how it is used in failure analysis. It reviews the basic types of fracture processes, namely, ductile, brittle, fatigue, and creep, principally in terms of fracture appearances, such as microstructure. The article also describes the general features of fatigue fractures in terms of crack initiation and fatigue crack propagation.

You do not currently have access to this content.
Don't already have an account? Register

W.T. Becker, S. Lampman, 2002. "Fracture Appearance and Mechanisms of Deformation and Fracture", Failure Analysis and Prevention, William T. Becker, Roch J. Shipley

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal