Failures of Bridge Components[1]

By
John W. Fisher
John W. Fisher
Fritz Engineering Laboratory, Lehigh University
Search for other works by this author on:
Published:
2002

Abstract

This article illustrates the defects, which result because of poor-quality welds in the bridge components. The cracks resulting from the use of low fatigue strength details are also discussed. The article describes the effect of out-of-plane distortion in floor-beam-girder connection plates, multiple-girder diaphragm connection plate, and tied-arch floor beams.

You do not currently have access to this content.
Don't already have an account? Register

John W. Fisher, 2002. "Failures of Bridge Components", Failure Analysis and Prevention, William T. Becker, Roch J. Shipley

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal