Skip to Main Content
ASM Handbook

Failure Analysis and Prevention

Edited by
William T. Becker
William T. Becker
Search for other works by this author on:
Roch J. Shipley
Roch J. Shipley
Search for other works by this author on:
ASM International
Volume
11
ISBN electronic:
978-1-62708-180-1
Publication date:
2002
Book Chapter

Fundamentals of Wear Failures

By
Raymond G. Bayer
Raymond G. Bayer
Tribology Consultant
Search for other works by this author on:
Published:
2002
Page range:
901 - 905
Publication history
November 01, 2002

Abstract

This article focuses on the types of activities required for the resolution of wear problems. These include examining and characterizing the tribosystem; characterizing and modeling the wear process; obtaining and evaluating wear data; and evaluating and verifying the solution.

You do not currently have access to this content.
Don't already have an account? Register

Raymond G. Bayer, 2002. "Fundamentals of Wear Failures", Failure Analysis and Prevention, William T. Becker, Roch J. Shipley

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal