Skip to Main Content
ASM Handbook

Welding Fundamentals and Processes

Edited by
T. Lienert
T. Lienert
Search for other works by this author on:
;
T. Siewert
T. Siewert
Search for other works by this author on:
;
S. Babu
S. Babu
Search for other works by this author on:
;
V. Acoff
V. Acoff
Search for other works by this author on:
ASM International
Volume
6A
ISBN electronic:
978-1-62708-174-0
Publication date:
2011
Book Chapter

Stud Arc Welding[1]

Published:
2011
Page range:
380 - 390
Publication history
April 07, 2011

Abstract

This article serves as a basic information source for those interested in accomplishing one-sided, no-hole attachment of metal fasteners. The stud arc-welding process is a substitute for fastening procedures such as drilling and tapping, bolting, and self-tapping screws. The article describes the operating principle of, and the tooling and equipment used for, the welding process. It contains tables that present information on the mechanical properties of aluminum, stainless steel, and low-carbon steel stud arc welded fasteners. The article details the different tests conducted to ensure the quality of stud arc-welded fasteners. It concludes with information on safety precautions to be followed in the welding process.

You do not currently have access to this content.
Don't already have an account? Register

2011. "Stud Arc Welding", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal