Laser Weld Quality Monitoring

By
Randolph Paura
Randolph Paura
Dynamic Laser Solutions
Search for other works by this author on:
Published:
2011
Page range:
595 - 605
Publication history
September 07, 2011

Abstract

This article reviews weld quality monitoring considerations for two automotive materials, steel and aluminum, with a focus on photosensor technology. It provides an overview of the process description, process parameters, and weld characteristics of laser welding. The article discusses real-time or in-process monitoring, which is done with optical, acoustic, and/or charged-particle sensors. It highlights the advantages, applications, and selection criteria of weld monitoring system and concludes with examples of laser weld monitoring in the production of tailor-welded blanks.

You do not currently have access to this content.
Don't already have an account? Register

Randolph Paura, 2011. "Laser Weld Quality Monitoring", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal