Skip to Main Content
ASM Handbook

Welding Fundamentals and Processes

Edited by
T. Lienert
T. Lienert
Search for other works by this author on:
T. Siewert
T. Siewert
Search for other works by this author on:
S. Babu
S. Babu
Search for other works by this author on:
V. Acoff
V. Acoff
Search for other works by this author on:
ASM International
Volume
6A
ISBN electronic:
978-1-62708-174-0
Publication date:
2011
Book Chapter

Gas Tungsten Arc Welding with Penetration-Enhancing Compounds

By
Ian D. Harris
Ian D. Harris
Edison Welding Institute
Search for other works by this author on:
Published:
2011
Page range:
355 - 358
Publication history
September 05, 2011

Abstract

This article describes compounds developed to enhance the penetration of the gas tungsten arc welding (GTAW) process. Penetration-enhanced GTAW processes have been referred to variously as Flux TIG, A-TIG, and GTAW with a penetration-enhancing compound (PEC). In all cases, the process uses a material that is not a flux but rather an oxide or mixture of oxides. The productivity of traditional GTAW is limited for many applications because of low deposition rates, shallow penetration (typically 3 mm, or ? in.), or inconsistent penetration. Penetration-enhanced GTAW processes can increases weld penetration by as much as 300% and reduces heat-to-heat variation in penetration and distortion.

You do not currently have access to this content.
Don't already have an account? Register

Ian D. Harris, 2011. "Gas Tungsten Arc Welding with Penetration-Enhancing Compounds", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal