Fluid Flow Phenomena during Welding[1]

By
W. Zhang
W. Zhang
Updating author
Oak Ridge National Laboratory
Search for other works by this author on:
Published:
2011
Page range:
89 - 95
Publication history
April 07, 2011

Abstract

Fluid flow is important because it affects weld shape and is related to the formation of a variety of weld defects in gas tungsten arc (GTA) welds. This article describes the surface-tension-driven fluid flow model and its experimental observations. The effects of mass transport on arc plasma and weld pool are discussed. The article reviews the strategies for controlling poor and variable penetration and describes the formation of keyhole and fluid flow in electron beam and laser welds. It also explains the fluid flow in gas metal arc welding and submerged arc welding, presenting its transport equations.

You do not currently have access to this content.
Don't already have an account? Register

W. Zhang, 2011. "Fluid Flow Phenomena during Welding", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal