Skip to Main Content
ASM Handbook

Welding Fundamentals and Processes

Edited by
T. Lienert
T. Lienert
Search for other works by this author on:
T. Siewert
T. Siewert
Search for other works by this author on:
S. Babu
S. Babu
Search for other works by this author on:
V. Acoff
V. Acoff
Search for other works by this author on:
ASM International
Volume
6A
ISBN electronic:
978-1-62708-174-0
Publication date:
2011
Book Chapter

Forge and Coextrusion Welding

By
Paul S. Korinko
Paul S. Korinko
Revising author
Savannah River National Laboratory
Search for other works by this author on:
Published:
2011
Page range:
701 - 703
Publication history
April 16, 2011

Abstract

Forge welding is a solid-state joining process in which the workpieces are heated to the welding temperature and then sufficient blows or force are applied to cause permanent deformation and bonding at the faying surfaces. Coextrusion welding is a solid-state process that produces a weld by heating two or more workpieces to the welding temperature and forcing them through an extrusion die. This article illustrates typical joint configurations used for manual and automatic forge welding applications. It provides information on the common metals welded by coextrusion welding, such as low-carbon steel, aluminum, copper, and copper alloys. The article also explains the common coextrusion behaviors.

You do not currently have access to this content.
Don't already have an account? Register

Paul S. Korinko, 2011. "Forge and Coextrusion Welding", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal