Book Chapter

Submerged Arc Welding

By
Lee E. Allgood
Lee E. Allgood
The Lincoln Electric Company
Search for other works by this author on:
Published:
2011
Page range:
335 - 343
Publication history
April 16, 2011

Abstract

Submerged arc welding (SAW) is suited for applications involving long, continuous welds. This article describes the operating principle, application, advantages, limitations, power source, equipment, and fluxes in SAW. It reviews three different types of electrodes manufactured for SAW: solid, cored, and strip. The article highlights the factors to be considered for controlling the welding process, including fit-up of work, travel speed, and flux depth. It also evaluates the defects that occur in SAW: lack of fusion, slag entrapment, solidification cracking, and hydrogen cracking. Finally, the article provides information on the safety measures to be followed in this process.

You do not currently have access to this content.
Don't already have an account? Register

Lee E. Allgood, 2011. "Submerged Arc Welding", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal