Skip to Main Content
ASM Handbook

Welding Fundamentals and Processes

Edited by
T. Lienert
T. Lienert
Search for other works by this author on:
T. Siewert
T. Siewert
Search for other works by this author on:
S. Babu
S. Babu
Search for other works by this author on:
V. Acoff
V. Acoff
Search for other works by this author on:
ASM International
Volume
6A
ISBN electronic:
978-1-62708-174-0
Publication date:
2011
Book Chapter

Modeling of Heat and Mass Transfer in Fusion Welding

By
Wei Zhang
Wei Zhang
Oak Ridge National Laboratory
Search for other works by this author on:
Rohit Rai
Rohit Rai
Pennsylvania State University
Search for other works by this author on:
Amit Kumar
Amit Kumar
ExxonMobil Upstream Research Company
Search for other works by this author on:
Igor V. Krivtsun
Igor V. Krivtsun
E.O. Paton Electric Welding Institute of the National Academy of Sciences of Ukraine
Search for other works by this author on:
Published:
2011
Page range:
766 - 788
Publication history
September 09, 2011

Abstract

This article provides a comprehensive review and critical assessment of numerical modeling of heat and mass transfer in fusion welding. The different fusion welding processes are gas tungsten arc welding, gas metal arc welding, laser welding, electron beam welding, and laser-arc hybrid welding. The article presents the mathematical equations of mass, momentum, energy, and species conservation. It reviews the applications of heat transfer and fluid flow models for different welding processes. Finally, the article discusses the approaches to improve reliability of, and reduce uncertainty in, numerical models.

You do not currently have access to this content.
Don't already have an account? Register

Wei Zhang, Rohit Rai, Amit Kumar, Igor V. Krivtsun, 2011. "Modeling of Heat and Mass Transfer in Fusion Welding", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff