Resistance Spot Welding

By
Murali D. Tumuluru
Murali D. Tumuluru
United States Steel Corporation
Search for other works by this author on:
Published:
2011
Page range:
409 - 422
Publication history
July 13, 2011

Abstract

Resistance spot welding (RSW) is the most widely used joining technique for the assembly of sheet metal products. This article discusses the process description, evaluation methods, and applications of RSW. It describes the equipment needed for RSW and explicates the major functions of electrodes in RSW and effect of surface condition on the technique. The article concludes with information on the safety precautions to be followed during the welding process.

You do not currently have access to this content.
Don't already have an account? Register

Murali D. Tumuluru, 2011. "Resistance Spot Welding", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal