Safe Welding Practices[1]

By
American Welding Society
American Welding Society
Search for other works by this author on:
Published:
2011
Page range:
845 - 868
Publication history
September 02, 2011

Abstract

This article presents an overview of the rules, regulations, and techniques implemented to minimize the safety hazards associated with welding, cutting, and allied processes. Safety management, protection of the work area, process-specific safety considerations, and robotic and electrical safety are discussed. The article explains the use of personal protective equipment and provides information on protection against fumes, gases, and electromagnetic radiation. It concludes with a discussion on safe handling of compressed gases as well as the prevention and protection of fire and explosion.

You do not currently have access to this content.
Don't already have an account? Register

American Welding Society, 2011. "Safe Welding Practices", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff