Skip to Main Content
ASM Handbook

Welding Fundamentals and Processes

Edited by
T. Lienert
T. Lienert
Search for other works by this author on:
T. Siewert
T. Siewert
Search for other works by this author on:
S. Babu
S. Babu
Search for other works by this author on:
V. Acoff
V. Acoff
Search for other works by this author on:
ASM International
Volume
6A
ISBN electronic:
978-1-62708-174-0
Publication date:
2011
Book Chapter

High-Frequency Welding[1]

By
Menachem Kimchi
Menachem Kimchi
Revising author
Edison Welding Institute
Search for other works by this author on:
Published:
2011
Page range:
456 - 462
Publication history
June 20, 2011

Abstract

High-frequency resistance welding (HFRW) is a process that uses high-frequency currents to concentrate the welding heat at the desired location. This article focuses on the fundamentals, advantages, limitations, and applications of HFRW. It discusses the personnel and equipment requirements as well as safety considerations necessary for the process. The article concludes with a discussion on the techniques for inspection and quality control of HFRW.

You do not currently have access to this content.
Don't already have an account? Register

Menachem Kimchi, 2011. "High-Frequency Welding", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal