Book Chapter

Introduction to High Energy Density Electron and Laser Beam Welding

By
J.W. Elmer
J.W. Elmer
Search for other works by this author on:
P.W. Hochanadel
P.W. Hochanadel
Search for other works by this author on:
K. Lachenberg
K. Lachenberg
Search for other works by this author on:
C. Caristan
C. Caristan
Search for other works by this author on:
T. Webber
T. Webber
Search for other works by this author on:
Published:
2011
Page range:
507 - 513
Publication history
September 02, 2011

Abstract

This article provides a history of electron and laser beam welding, discusses the properties of electrons and photons used for welding, and contrasts electron and laser beam welding. It presents a comparison of the electron and laser beam welding processes. The article also illustrates constant power density boundaries, showing the relationship between the focused beam diameter and the absorbed beam power for approximate regions of keyhole-mode welding, conduction-mode welding, cutting, and drilling.

You do not currently have access to this content.
Don't already have an account? Register

J.W. Elmer, P.W. Hochanadel, K. Lachenberg, C. Caristan, T. Webber, 2011. "Introduction to High Energy Density Electron and Laser Beam Welding", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff