Ultrasonic Welding

By
Janet Devine
Janet Devine
Sonobond Ultrasonics Inc.
Search for other works by this author on:
Published:
2011
Page range:
725 - 730
Publication history
July 27, 2011

Abstract

Ultrasonic metal welding is a solid-state welding process that produces coalescence through the simultaneous application of localized high-frequency vibratory energy and moderate clamping forces. This article discusses the parameters to be considered when selecting a suitable welder for ultrasonic metal welding. It details the personnel requirements, advantages, limitations, and applications, namely, wire welds, spot welds, continuous seam welds, and microelectronic welds of ultrasonic metal welding.

You do not currently have access to this content.
Don't already have an account? Register

Janet Devine, 2011. "Ultrasonic Welding", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff