Friction Surfacing[1]

Published:
2011
Page range:
678 - 681
Publication history
April 12, 2011

Abstract

The friction surfacing process enables deposition of a wide variety of high-specification materials with an ideal metallurgical bond onto a range of metal substrates. This article provides a process description and discusses the equipment used for, and the applications of, friction surfacing.

You do not currently have access to this content.
Don't already have an account? Register

2011. "Friction Surfacing", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal