Book Chapter

An Overview of Joining Processes

By
Robert W. Messler, Jr.
Robert W. Messler, Jr.
Rensselaer Polytechnic Institute
Search for other works by this author on:
Published:
2011
Page range:
3 - 12
Publication history
April 05, 2011

Abstract

Joining is key to the manufacture of large or complex devices or assemblies; construction of large and complex structures; and repair of parts, assemblies, or structures in service. This article describes the three forces for joining: physical, chemical, and mechanical. It provides an overview of the joining processes, namely, mechanical fastening, integral attachment, adhesive bonding, welding, brazing, and soldering. The article concludes with information on the various aspects of joint design and location that determine the selection of a suitable joining method.

You do not currently have access to this content.
Don't already have an account? Register

Robert W. Messler, Jr., 2011. "An Overview of Joining Processes", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff