Skip to Main Content
ASM Handbook

Welding Fundamentals and Processes

Edited by
T. Lienert
T. Lienert
Search for other works by this author on:
T. Siewert
T. Siewert
Search for other works by this author on:
S. Babu
S. Babu
Search for other works by this author on:
V. Acoff
V. Acoff
Search for other works by this author on:
ASM International
Volume
6A
ISBN electronic:
978-1-62708-174-0
Publication date:
2011
Book Chapter

Resistance Welding Power Supplies and Controls

By
Donald F. Maatz, Jr.
Donald F. Maatz, Jr.
RoMan Engineering Services
Search for other works by this author on:
Tom Morrissett
Tom Morrissett
RoMan Engineering Services
Search for other works by this author on:
Published:
2011
Page range:
404 - 408
Publication history
May 23, 2011

Abstract

This article provides an overview of the components of a resistance welding machine. It focuses on the single-phase control system and medium-frequency direct current system of resistance welding. The article also includes information on their feedback systems, rectification systems, and power sources.

You do not currently have access to this content.
Don't already have an account? Register

Donald F. Maatz, Jr., Tom Morrissett, 2011. "Resistance Welding Power Supplies and Controls", Welding Fundamentals and Processes, T. Lienert, T. Siewert, S. Babu, V. Acoff

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal