Skip to Main Content
ASM Handbook

Casting

Edited by
Srinath Viswanathan
Srinath Viswanathan
Search for other works by this author on:
Diran Apelian
Diran Apelian
Search for other works by this author on:
Raymond J. Donahue
Raymond J. Donahue
Search for other works by this author on:
Babu DasGupta
Babu DasGupta
Search for other works by this author on:
Michael Gywn
Michael Gywn
Search for other works by this author on:
John L. Jorstad
John L. Jorstad
Search for other works by this author on:
Raymond W. Monroe
Raymond W. Monroe
Search for other works by this author on:
Mahi Sahoo
Mahi Sahoo
Search for other works by this author on:
Thomas E. Prucha
Thomas E. Prucha
Search for other works by this author on:
Daniel Twarog
Daniel Twarog
Search for other works by this author on:
ASM International
Volume
15
ISBN electronic:
978-1-62708-187-0
Publication date:
2008
Book Chapter

Expandable-Mold Casting Processes with Permanent Patterns

Published:
2008

Abstract

Casting can be done with either expendable molds for one-time use or permanent molds for reuse many times. This article lists various methods used to fabricate expendable molds from permanent patterns. The methods include molding of sand with clay, inorganic binders, or organic resins; shell molding of sand with a thin resin-bonded shell; no-bond vacuum molding of sand; plaster-mold casting; ceramic-mold casting; rammed graphite molding; and magnetic (no-bond) molding of ferrous shot. The article tabulates a general comparison of casting methods and discusses the basic requirements of foundry molds.

Abstract

This article reviews the basic types of mold aggregates and bonding methods for expendable molds and coremaking. It provides an overview of mold media and the basic types of sands and their properties. The most significant clays used in green sand operations, such as bentonites, are discussed. The article describes the methods of sand bonding with inorganic compounds. It provides a description of resin-bonded sand systems, namely, no-bake binder systems, heat-cured binder systems, and cold box binder systems. The article concludes with a discussion on the media used for expendable molds, namely, ceramic shells and rammed graphite, for casting reactive metals such as titanium or zirconium.

You do not currently have access to this content.
Don't already have an account? Register

2008. "Expandable-Mold Casting Processes with Permanent Patterns", Casting, Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal