Skip to Main Content
ASM Handbook

Casting

Edited by
Srinath Viswanathan
Srinath Viswanathan
Search for other works by this author on:
Diran Apelian
Diran Apelian
Search for other works by this author on:
Raymond J. Donahue
Raymond J. Donahue
Search for other works by this author on:
Babu DasGupta
Babu DasGupta
Search for other works by this author on:
Michael Gywn
Michael Gywn
Search for other works by this author on:
John L. Jorstad
John L. Jorstad
Search for other works by this author on:
Raymond W. Monroe
Raymond W. Monroe
Search for other works by this author on:
Mahi Sahoo
Mahi Sahoo
Search for other works by this author on:
Thomas E. Prucha
Thomas E. Prucha
Search for other works by this author on:
Daniel Twarog
Daniel Twarog
Search for other works by this author on:
ASM International
Volume
15
ISBN electronic:
978-1-62708-187-0
Publication date:
2008
Book Chapter

Quality Planning Tools and Procedures

By
Alan Richardson
Alan Richardson
SPX Corporation
Search for other works by this author on:
Published:
2008
Page range:
1207 - 1212
Publication history
May 19, 2008

Abstract

The basic quality analysis tools are cause-and-effect diagrams, check sheets, control charts, histograms, Pareto charts, scatter diagrams, and run charts. This article reviews how the basic quality analysis tools are built upon to become a more advanced set of quality tools. It describes the advanced quality tools: advanced product quality planning, failure mode and effects analysis, control planning, measurement systems analysis, lean tools, statistical process control, production viability and tryout, and Six Sigma.

You do not currently have access to this content.
Don't already have an account? Register

Alan Richardson, 2008. "Quality Planning Tools and Procedures", Casting, Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal